Tests Average Test Results
Crazing Test Completely Craze Proof
Water Absorption Less Than 0.5 %
Modulus Of Rupture More Than 625 Kg/Sq. Cm
Chemical Resistance HIghly Resistant
Resistance To Staining And Burning Stain And Burn Proof